ASTM A312 Rørdimensioner i rustfrit stål

ASTM A312 rustfri stålrørdimensioner er fastsat af ANSI ASME B36.19-specifikationen.

 

ASTM A312 Rørvægt

Nominel rørstørrelse Udvendig diameter Rustfri stålrør Dimensioner
Skema 5S Skema 10S Skema 40S Skema 80S
(mm) (tommer) WT / VÆGT
mm (tommer) kg/m mm (tommer) kg/m mm (tommer) kg/m mm (tommer) kg/m
1/8 10.3 0.405 1.25 (0.049) 0.28 1.73 (0.068) 0.37 2.42 (0.095) 0.47
1/4 13.7 0.540 1.66 (0.065) 0.49 2.24 (0.088) 0.63 3.03 (0.119) 0.80
3/8 17.2 0.675 1.66 (0.065) 0.63 2.32 (0.091) 0.85 3.20 (0.126) 1.10
1/2 21.3 0.840 1.65 (0.065) 0.81 2.11 (0.083) 1.00 2.77 (0.109) 1.27 3.74 (0.147) 1.62
3/4 26.7 1.050 1.65 (0.065) 1.02 2.11 (0.083) 1.28 2.87 (0.113) 1.68 3.92 (0.154) 2.20
1 33.4 1.315 1.65 (0.065) 1.30 2.77 (0.109) 2.09 3.38 (0.133) 2.50 4.55(0.179) 3.24
1 1/4 42.2 1.660 1.65 (0.065) 1.66 2.77 (0.109) 2.69 3.56 (0.140) 3.39 4.86 (0.191) 4.47
1 1/2 48.3 1.900 1.65 (0.065) 1.91 2.77 (0.109) 3.11 3.69 (0.145) 4.06 5.08 (0.200) 5.41
2 60.3 2.375 1.65 (0.065) 2.40 2.77 (0.109) 3.93 3.92 (0.154) 5.45 5.54 (0.218) 7.49
2 1/2 73.0 2.875 2.11 (0.083) 3.69 3.05 (0.120) 5.26 5.16 (0.203) 8.64 7.01 (0.276) 11.4
3 88.9 3.500 2.11 (0.083) 4.52 3.05 (0.120) 6.46 5.49 (0.216) 11.3 7.62 (0.300) 15.3
3 1/2 101.6 4.000 2.11 (0.083) 5.18 3.05 (0.120) 7.41 5.74 (0.226) 13.6 8.08 (0.318) 18.6
4 114.3 4.500 2.11 (0.083) 5.84 3.05 (0.120) 8.37 6.02 (0.237) 16.1 8.56 (0.337) 22.3
5 141.3 5.563 2.77 (0.109) 9.46 3.41 (0.134) 11.6 6.56 (0.258) 21.8 9.53 (0.375) 31.0
6 168.3 6.625 2.77 (0.109) 11.3 3.41 (0.134) 13.9 7.12 (0.280) 28.3 10.9 (0.432) 42.6
8 219.1 8.625 2.77 (0.109) 14.8 3.76 (0.148) 20.0 8.18 (0.322) 42.5 12.7 (0.500) 64.6
10 273.1 10.750 3.41 (0.134) 22.7 4.20 (0.165) 27.8 9.28 (0.365) 60.4 12.7 (0.500) 81.5
12 323.9 12.750 3.97 (0.156) 31.3 4.58 (0.180) 36.1 9.53 (0.375) 73.9 12.7 (0.500) 97.4

 

ASTM A312 Rørdiametertolerance

NPS ASTM A312/ASME SA312 OD Tolerance
+
tomme Mm tomme Mm
1/8 til 1 1 /2
>1 1 /2 til 4
>4 til 8
>8 til 18
>18 til 26
>26 til 34
>34 til 48
1/64(0.015)
1/32(0.031)
1/16(0.062)
3/32(0.093)
1/8(0.125)
5/32(0.156)
3/16(0.187)
0.4
0.8
1.6
2.4
3.2
4.0
4.8
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
1/32(0.031)
0.8
0.8
0.8
0.8
0.8
0.8
0.8

 

ASTM A312 Rørvægtykkelsestolerance

Den nominelle vægtykkelsestolerance er +/- 12,5 %.

NPS ASTM A312/ASME SA312 WT Tolerance, %
+
1/8-2 1 /2 20.0 12.5
3~18, t/D Mindre end eller lig med 5 % 22.5 12.5
3~18, t/D> 5% 15.0 12.5
Større end eller lig med 20, svejset 17.5 12.5
Større end eller lig med 20, sømløs, t/D Mindre end eller lig med 5 % 22.5 12.5
≥ 20, seamless, t/D> 5% 15.0 12.5

 

 